Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cardia Compostable B-F12 - (PSAC+Polyester) - Cardia Bioplastics

Material Data Center offers the following functions for Cardia Compostable B-F12:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cardia Compostable datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
For more detailed information, please read our brochure p. 46 to 54
or contact our representatives in your region.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 2.55 g/10min ASTM D 1238
Température 190 °C -
Charge 2.61 kg -
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
Température de fusion 94 °C ASTM D 3418
Propriétés diversesValeurUnitéNorme du test
Densité 1200 kg/m³ ASTM D 792
Moisture Content 0.6 % -
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ASTM Data
Module en traction, long. 220 MPa ASTM D 882
Module en traction, trav. 140 MPa ASTM D 882
Module de traction, long. 28 MPa ASTM D 882
Module de traction, trav. 22 MPa ASTM D 882
Allongement à la rupture, long. 270 % ASTM D 882
Allongement à la rupture, trav. 470 % ASTM D 882
Type d'extrusion soufflage - -
Epaisseur des eprouvettes 0.02 mm -
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Type of extrusion blown - -
Température - Zone d'alimentation 120 - 150 °C -
Zone 1 130 - 160 °C -
Zone 2 140 - 165 °C -
Zone 3 140 - 165 °C -
Température de la buse 135 - 165 °C -
Caractéristiques
Transformation
Extrusion a film soufflé, Extrusion de films
Conditionnement
Noir, Marron, Couleurs naturelles
Additifs
Plastifiant
Certifications
Contient des ressources renouvelables, Biodégradables, Contact alimentaire, Compostable ISO 13432 (producteur), Compostable ASTM D6400 (producteur), Compostable ISO 13432 (certificat), Compostable ASTM D6400 (certificat)
Applications
Emballage
Disponibilité régionale
Amérique du nord, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.